An in-house investigation team from Equinor has studied the deviation in quality of welding and inspection of the Johan Castberg production vessel’s hull currently under construction at the Sembcorp Marine yard in Singapore.
The Johan Castberg (formerly Skrugard) field is situated approximately 100 kilometres north of the Snøhvit-field in the Barents Sea, located off the northern coast of Norway. The resource base consists of the three oil discoveries Skrugard, Havis and Drivis, located in PL 532 and is expected to come on stream in 2023, to produce for 30 years.
The field is planned to be developed with an FPSO vessel with additional subsea solutions.
The vessel’s hull is under construction in Singapore, the turret is being built in Dubai and the topside is being constructed in Stord, Norway. But during construction of the hull, Equinor reported that there were deviations for both welding and welding inspection.
The company announced this week that extensive work is being conducted to quality assure and cross-check welds and repair welding defects, to ensure that the vessel meets applicable safety and integrity requirements before leaving the yard.
Equinor’s senior vice president for project development, Geir Tungesvik, said the extensive cross-checking and repair of welds will ensure that the production vessel meets safety and integrity requirements.
“When Johan Castberg comes on stream, there should be no doubt that the vessel is safe,” said Tungesvik.
The yard is responsible for correcting all deviations in quality and costs related to repair of welding defects are covered by Sembcorp Marine, according to the contract. The cross-checks and improvements are almost completed and are followed up closely by Equinor.
“To ensure learning and avoid similar situations in other projects or at other yards, we have carried out a thorough investigation,” advised Tungesvik.
The investigation team did not find any single event which could have been a direct cause for the welding quality issues, but have pointed out causal factors considered as having had an impact:
- Contractor (SCM) failed to provide sufficient competent welders and welding inspectors for execution of the scope and did not sufficiently comply with processes and work routines for execution and follow up of welding and inspection activities.
- Equinor has not sufficiently complied with its own work processes and procedures for risk management, construction management and follow-up at the construction site.
- Even if Equinor’s follow-up team found signs of poor quality at an early stage, the extent and degree of seriousness were not understood. Sufficient measures were therefore not implemented.
- Equinor’s follow-up team has not had enough personnel with experience and expertise in welding and welding control and has not utilised the company’s technical expertise in these areas early enough.
“We are preparing a plan with specific actions to follow up the findings and we will share our experience,” said Tungesvik.
The investigation team has studied the causes of the deviations in welding quality in the period from January 2017 to October 2019. Based on this work the team recommends Equinor to improve:
- the prequalification process for new suppliers
- the practice for follow-up at construction sites, including risk management
- the recruitment process for follow-up teams and team composition

Illustration of the Johan Castberg production vessel, credit: Equinor ASA.
Extensive control and improvement
When Equinor, in the summer of 2019, cross-checked Sembcorp’s ultrasonic inspection of welds in the moonpool area of the hull by using own personnel, they discovered a higher failure rate than reported. It was then decided to cross-check all assembly welds. Unusually high failure rates in fabrication welds were revealed later.
“We have therefore reassessed all structural welds on the hull. This is a very demanding job as the hull has already been built, however safety comes first. The vessel must meet the requirements incorporated in the plan for development and operation (PDO) and obtain a DNV class certificate before sailing to the field,” said Tungesvik.
A reassessment of all structural welds has been made and extensive cross-checking is being carried out by use of non-destructive testing (NDT), including ultrasound.
“Equinor should have discovered the extent of welding defects earlier, however the hull is still in dock, allowing us to repair the defects before it is launched,” added Tungesvik.
The hull for the Johan Castberg production vessel is scheduled to be transported to Stord on board the Boka Vanguard heavy-lift vessel late 2021, however the COVID-19 pandemic still adds uncertainty to all schedules.
Licence partners in Johan Castberg include Equinor Energy AS (operator) 50 per cent, Vår Energi AS 30 per cent and Petoro AS 20 per cent.